Pipa Baja Seamless ASTM A106 Gr.B

Katrangan singkat:

ASTM A106 / ASME SA106 minangka spesifikasi standar kanggo pipa baja karbon sing mulus kanggo aplikasi suhu dhuwur.Iku kasusun saka telung gelar A, B lan C, kelas umum digunakake A106 kelas B. Iku ora mung digunakake ing sistem pipa kayata lenga lan gas, banyu, lan transportasi slurry, nanging uga ing boiler, construction lan aplikasi struktural.


Detail Produk

Tag produk

Pambuka produk

Pipa ASTM A106 Grade B kanthi kimia padha karo ASTM A53 Grade B lan API 5L Grade B ing babagan posisi kimia lan sifat mekanik, umume nggunakake baja karbon, kanthi kekuatan ngasilake minimal 240 MPa lan kekuatan tarik 415 MPa.

Spesifikasi Standar ASTM A106 kanggo Pipa Baja Seamless duwe telung gelar, kelas ASTM A106 Gr.A.B lan C, sing luwih dhuwur bahan bahan, luwih apik sifat kekuatan.

Tampilan produk

ASTM A106 Gr.B Baja Seamless 4
ASTM A106 Gr.B Baja Seamless 2
ASTM A106 Gr.B Baja Seamless 1

Metode Pengujian

Cara tes kanggo ASTM A106 A, B, C yaiku tes flattening, tes listrik sing ora ngrusak, tes ultrasonik, tes arus eddy, tes bocor fluks magnetik, prosedur tes kasebut kudu dilaporake utawa dirembug karo pelanggan kanggo nemtokake tes sing bakal ditindakake. digunakake.

Standar: ASTM A106, Nace, Sour service.

Kelas: A, B, C

Kisaran diameter njaba OD: NPS 1/8 inci nganti NPS 20 inci, 10,13mm nganti 1219mm.

Kisaran kekandelan tembok WT: SCH 10, SCH 20, SCH STD, SCH 40, SCH 80, kanggo SCH160, SCHXX;1.24mm nganti 1 inci, 25.4mm.

Range saka dawa: 20ft kanggo 40ft, 5,8m kanggo 13m, siji acak dawa 16 kanggo 22ft, 4,8 kanggo 6,7m, pindho dawa acak karo rata-rata 35ft 10,7m.

Prosesi pungkasan: Ujung polos, miring, benang.

Lapisan: Cat ireng, varnished, lapisan epoksi, lapisan poliethelin, FBE lan 3PE, CRA Klambi lan Diantrekake.

Komposisi Kimia (%)

sasmita

C≤

Mn

P≤

S≤

Si≥

Cr≤

Cu≤

Mo≤

Ni≤

V≤

A

0.25

0.27-0.93

0.035

0.035

0.1

0.4

0.4

0.15

0.4

0.08

B

0.3

0.29-1.06

0.035

0.035

0.1

0.4

0.4

0.15

0.4

0.08

C

0.35

0.29-1.06

0.035

0.035

0.1

0.4

0.4

0.15

0.4

0.08

Sifat Mekanik

sasmita Rm Mpa Kekuwatan Tarik Titik Hasil (Mpa) Elongation Kahanan Pangiriman
A ≥330 ≥205 20 Annealed
B ≥415 ≥240 20 Annealed
C ≥485 ≥275 20 Annealed

Toleransi Dimensi

Tipe Pipa

Ukuran Pipa

Toleransi

Digambar Dingin

OD

≤48.3mm

± 0,40 mm

≥60.3mm

± 1% mm

WT

± 12,5%